There may be some problems when taking silicon rubber mould such as SiliconeRubber For Tire Mold Making.
Delamination occurs after the molds are removed
Possible cause: the first impression is contaminated with saliva or blood
Countermeasure: clean and dry the first printing die
Angular defect occurs after the die is removed
Possible reason: the tray is placed too fast
Countermeasure: tray is placed slowly
Position error (correction printing technology)
Possible reason: the first printing die was not placed in the original position when it was placed again
Countermeasures: determine the first printing die in the correct position (can be marked in advance)
D. Second printing mode pre-curing (double mixing technology)
Possible reason: the high temperature in the oral cavity causes the pre-placed secondary impression mold to solidify before the tray is placed in the oral cavity
Countermeasure: make sure the tray is placed in the mouth before the second printing mold has not solidified